There is provided a glass enamel system adaptable to be fired from about 1000° F. to about 1350° F., said glass enamel characterized, upon firing, by a formation therein of metal orthosilicate crystals, which has the effect of substantially hardening the surface of said glass enamel even at its fusion point temperature, and within the range aforesaid.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 21.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A glass enamel system, the glass fraction of which is a lead borosilicate glass, wherein said system is adaptable to be fired and fused to a glass enamel on a glass substrate at from about 1000° F. to about 1350° F., comprising a crystallizing amount dispersed in said system of the precursors of the crystal Cd 2 SiO 4 in sufficient quantities to provide from about 25 to about 50 weight percent Cd 2 SiO 4 in the resulting, fired enamel.

  2. Claim 2Depends on #1

    The glass enamel system of claim 1 wherein essentially all the precursors of Cd 2 SiO 4 are present in the form of crystalline Cd 2 SiO 4 .

  3. Claim 3Depends on #1

    The glass enamel system of claim 1 wherein the precursors of Cd 2 SiO 4 are present as CdO and SiO 2 , in solution in a cadmium borosilicate glass frit as a component of said glass enamel system.