Abstract
In order to reduce the water content in piezoelectric GaPO 4 crystal elements the proposal is put forward that each GaPO 4 crystal element should be cut in its entirety from one uniform growth zone of a GaPO 4 raw crystal bar and should not contain any zone boundaries, and that the piezoelectric GaPO 4 crystal elements should be treated with a dehydrating solution, until an infrared coefficient of α<1.5 cm -1 is obtained at a wavelength in the vicinity of 2.0 μm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of reducing the water content in piezoelectric GaPO 4 crystal elements, wherein each of said piezoelectric GaPO 4 crystal elements is cut entirely from one uniform growth zone of a GaPO 4 raw crystal bar, and is free of any zone boundaries.
- Claim 2Independent Claim
A method of reducing the water content in piezoelectric GaPO 4 crystal elements, wherein said piezoelectric GaPO 4 crystal elements are treated with a dehydrating solution until an infrared coefficient of α<1.5 cm -1 is obtained at a wavelength of approximately 2.9 μm, with α=1/d log (I.sub.o /I) I o : intensity of primary radiation I: intensity of transmission radiation d: thickness of said crystal element.
- Claim 3Depends on #2
A method according to claim 2, wherein said infrared coefficient α is less than 0.8 cm -1 .
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.