Method of preparing an asbestos diaphragm
Abstract
An electrolyte permeable asbestos diaphragm is prepared by depositing asbestos and a particulate thermoplastic polymeric material from an aqueous slurry including alkali metal hydroxide onto a porous substrate, and heating the deposited asbestos, particulate thermoplastic polymeric material, and alkali metal hydroxide for a period of time, e.g., at least 2 hours, and at temperatures sufficient to react the asbestos and alkali metal hydroxide but temperatures insufficient to melt or sinter the particulate thermoplastic polymeric material, whereby the particulate thermoplastic polymeric material functions to provide permeability for the diaphragm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of depositing a liquid permeable asbestos diaphragm on a foraminous cathode structure by the steps of: (a) providing an aqueous slurry containing from about 100 to about 200 grams per liter alkali metal hydroxide and from about 0.5 to about 3 weight percent, basis total weight of slurry, of asbestos and particulate alternating copolymer of ethylene and chlorotrifluoro-ethylene, the copolymer being present in amount of from about 1 to about 30 weight percent basis total weight of asbestos and copolymer; (b) contacting a foraminous cathode structure with the slurry so as to deposit on
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗