Stabilization of poly(arylene ether ketones)
Abstract
A method of stabilizing a poly(arylene ether ketone), which method comprises in one embodiment heating the poly(arylene ether ketone) at a temperature between about 240° C. and about 325° C. for a period of between about 0.5 and about 24 hours, prior to any melt-processing of the poly(arylene ether ketone) and in another embodiment hydrothermally treating the poly(arylene ether ketone) by heating it to a temperature of at least 160° C. while contacting it with water.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 38.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of stabilizing a poly(arylene ether ketone), comprising heating the poly(arylene ether ketone) at a temperature between about 240° C. and about 325° C. for a period of between about 0.5 and about 24 hours, prior to any melt-processing of the poly(arylene ether ketone).
- Claim 2Depends on #1
A method according to claim 1, wherein the heating is performed in an air or nitrogen atmosphere.
- Claim 3Depends on #1
A method according to claim 1, wherein the heating is performed under a vacuum.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 38 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (1)
- Attwood et al, Polymer 22, 1096 (1981).