Patents
US 4,874,569 A#5623438 Most CitedExpiredUnited States (USPTO)Utility

Ceramic composite and methods of making the same

16Forward Citations (#5623438 Global)
0.4/yrCitation Velocity (#18588753 Global)
3.95Citation PageRank (#4869285 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There is provided a method for producing a self-supporting ceramic composite comprising (1) a ceramic matrix obtained by oxidation of an aluminum zinc alloy to form a polycrystalline oxidation reaction product of the metal with an oxidant, and (2) one or more fillers embedded by the matrix. The metal alloy and permeable mass of filler having at least one defined surface boundary are oriented relative to each other so that formation of the oxidation reaction product will occur into said mass of filler and in a direction towards said defined surface boundary. On heating the metal to a first temperature above its melting point but below the melting point of said oxidation reaction product to form a body of molten parent metal, the molten metal reacts with said oxidant to form said oxidation reaction product which infiltrates said mass of filler to said defined surface boundary. The resulting infiltrated mass is heated to a second temperature in order to remove or oxidize at least a substantial portion of any residual non-oxidized metallic constituents from or in said infiltrated mass without substantial formation of said oxidation reaction product beyond said defined surface boundary,

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 16.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a self-supporting ceramic composite comprising (1) a ceramic matrix obtained by oxidation of a parent metal comprising an aluminum alloy to form a polycrystalline material comprising an oxidation reaction product of the parent metal with at least one oxidant; and (2) at least one filler embedded by the matrix, which method comprises: (a) positioning a parent metal, comprising an aluminum alloy having at least about 1% by weight zinc, adjacent to a permeable mass of filler having at least one defined surface boundary and orienting said parent metal and said filler relativ

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • "Oxidation of Molten Aluminum Alloys. Reaction with Refractories"--M. Drouzy and M. Richard--Mar., 1974--Fonderie, France No. 332, pp. 121-128.
  • "Refractories for Aluminum Alloy Melting Furnaces"--B. Clavaud and V. Jost--Sep., 1980--Lillian Brassinga (from French), Jan. 1985.
  • Oxidation of Molten Aluminum Alloys. Reaction with Refractories M. Drouzy and M. Richard Mar., 1974 Fonderie, France No. 332, pp. 121 128.
  • Refractories for Aluminum Alloy Melting Furnaces B. Clavaud and V. Jost Sep., 1980 Lillian Brassinga (from French), Jan. 1985.