Patents
US 4,867,931 A#993953 Most CitedExpiredUnited States (USPTO)Utility

Methods for producing fiber reinforced microspheres made from dispersed particle compositions

48Forward Citations (#993953 Global)
1.3/yrCitation Velocity (#4458524 Global)
13.29Citation PageRank (#661082 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Fiber reinforced hollow microspheres made from dispersed particle film forming compositions including fibers, dispersed particles, a binder, a film stabilizing agent, a dispersing agent and a continuous liquid phase. Porous and non-porous fiber reinforced hollow microspheres can be made. The fiber reinforced hollow microspheres have walls with voids which are interconnected to each other and to the inner and outer wall surfaces, and the fiber reinforced hollow microspheres can be used as membrane substrates in selective separation processes and in biotech processes. The fiber reinforced hollow microspheres can be used as supports for catalysts and as enclosures for catalysts, adsorbents and absorbents. The fiber reinforced hollow microspheres can also be used as filler materials and as proppants for increasing gas recovery from gas wells. The fiber reinforced hollow microspheres are made by a process which includes forming a film of a fiber and dispersed particle film forming composition across a coaxial blowing nozzle, applying a blowing gas at a positive pressure on the inner surface of the fiber and dispersed particle composition film to blow the film and form an elongated cylin

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 48.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for making fiber reinforced hollow porous microspheres of 200 to 10,000 microns diameter and of 1 to 1000 microns wall thickness from a stable dispersion of a fiber and dispersed particle film forming composition, said composition comprising fibers and dispersed particles in a continuous liquid phase, wherein said fibers have a diameter of 0.5 to 10 microns and a length of 2 to 500 microns and the ratio of fiber diameter to length is 1:3 to 1:100 said method comprising feeding said fibers and dispersed particle composition and a blowing gas to a coaxial blowing nozzle, said coaxial bl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗