Heat treatment of rapidly quenched Fe-6.5 wt % Si ribbon

19Forward Citations (#4553485 Global)
0.5/yrCitation Velocity (#15127158 Global)
3.23Citation PageRank (#6716973 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A rapidly quenched Fe-Si alloy containing 6 to 7 wt % Si is heat treated to promote and control an order-disorder reaction, thereby improving its ac core loss and exciting power at induction levels above B=1.2 T. The alloy has a substantially <100> texture, a grain size of about 1 to 2 mm, a B2 domain size of 100 to 850 nm, a DO3 domain size of about 5 to 25 nm, an ac core loss of about 1.2 to 1.6 W/kg and an exciting power of about 15 to 46 VA/kg, the core loss and exciting power being measured at an induction level of B=1.4 T and a frequency of f=60 Hz.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 19.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of heat treatment for Fe-Si alloys consisting of Fe and 6 to 7 wt % Si when rapidly quenched from a melt, which method promotes an order-disorder reaction, thereby improving the magnetic properties at high induction levels, comprising the steps of: vacuum annealing at a temperature between 1000° C. and 1200° C. for 1 to 4 hours to develop a grain size in the range of 1-2 nm, and a strong <100> texture with intensity at least 2 times that of a reference sample having a randomly oriented grain structure; and annealing at a temperature between 790° C. and 860° C. for 1 to 4 hours

  2. Claim 2Depends on #1

    A method of heat treatment as recited in claim 1, wherein said vacuum annealing step is performed at a temperature b

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 19 total)

Non-Patent Literature (5)

  • "Rapidly Solidified Materials,"0 ed. by P. W. Lee and R. S. Carbonara, pp. 273-281. American Society for Metals, Ohio (1986).
  • Arai et al., "Grain Growth of Rapid Quenching High Silicon Iron Alloys", IEEE Trans. on Magnetics, vol. MAG 5, Sep. 1984, pp. 1463-1465.
  • Arai et al., Grain Growth of Rapid Quenching High Silicon Iron Alloys , IEEE Trans. on Magnetics, vol. MAG 5, Sep. 1984, pp. 1463 1465.
  • C. F. Chang, R. L. Bye, V. Laxmanan, S. K. Das. "Texture and Magnetic Properties of Rapidly Quenched Fe-6.5 wt. % Si Ribbon." Transactions on Magnetics, vol. MAG-20, No. 4, Jul. 1984, pp. 553-558.
  • C. F. Chang, R. L. Bye, V. Laxmanan, S. K. Das. Texture and Magnetic Properties of Rapidly Quenched Fe 6.5 wt. % Si Ribbon. Transactions on Magnetics, vol. MAG 20, No. 4, Jul. 1984, pp. 553 558.