Patents
US 4,863,669 A#11189439 Most CitedExpiredUnited States (USPTO)Utility

Process for forming polyarylenethioether stretched blow-molded vessel

9Forward Citations (#11189439 Global)
0.2/yrCitation Velocity (#30270635 Global)
2.78Citation PageRank (#8554430 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for forming a polyarylenethioether stretched blow molded vessel, by a modified blow molding of a substantially linear polyarylenethioether having a melt viscosity of 3,000 to 20,000 poise [at 310 DEG C., shear rate=200 sec-1]. The modified blow molding involves injecting the polymer in a mold to form a bottomed parison, stretching the bottomed parison along its axis by means of a rod or mandrel, and the stretched bottomed parison is then subjected to blow molding to effect lateral stretching. The blow parison is then heat set.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a polyarylenethioether stretched blow-molded vessel, which comprises injecting a substantially linear polyarylenethioether having a melt viscosity of 3,000 to 20,000 poise measured at 310° C. and a shear rate of 200 sec -1 into a mold of 0° to 130° to form a bottomed parison with an opening at an opposite end, pushing a rod into said bottomed parison through the opening thereof to stretch the parison at a resin temperature of 80° to 150° C. in the longitudinal direction of 1.5 to 6-fold, subsequently blowing a gas into the parison at a resin temperature of 90° to 180°

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗