Patents
US 4,863,635 A#24147661 Most CitedExpiredUnited States (USPTO)Utility

Method of treating the surface of polymers with a cuprous compound to form a copper sulfide composite structure

4Forward Citations (#24147661 Global)
0.1/yrCitation Velocity (#43650388 Global)
1.48Citation PageRank (#23430274 Global)
4Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for making a conductive polymer for static charge dissipation, electromagnetic induction shielding, electroplating, or making a semiconductor comprises uniformly mixing into any number of polymer or polymer blends which are in a molten or semimolten state about 1 to about 30% by weight of sulfur to form a polymer/sulfur blend. Once the polymer/sulfur blend is solidified, by cooling, it is exposed to an aqueous cuprous ion solution whereby the cuprous ions react with the sulfur in the polymer/sulfur blend to form copper sulfide dendrites within the polymer. The aqueous cuprous ion solution may also contain elemental sulfur to aid in the formation of the copper sulfide. Additionally, the aqueous cuprous ion solution may also contain an effective amount of dilute hydrochloric acid or dilute ammonium hydroxide to aid in the facilitation of complexation. The conductive polymers of the present invention have a resistivity of less than about 10,000 ohms/sq. and preferably less than about 400 ohms/sq.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A conductive polymer useful for static charge dissipation, electromagnetic induction shielding, and electroplating consisting essentially of: (a) a blend of a polymer, and (b) a sufficient amount of dendritic copper sulfide within said polymer so that said polymer has a resistivity of below about 10,000 ohms/sq.

  2. Claim 2Independent Claim

    A method for making a conductive polymer for static charge dissipation, electromagnetic induction shielding, and electroplating comprising: (a) uniformly mixing into a molten or semi-molten polymer 1 to 30% by weight of elemental sulfur to form a polymer/sulfur blend; (b) cooling said polymer/sulfur blend until it solidifies; and (c) exposing said solidified polymer/sulfur blend to an aqueous cuprous ion solution at a temperature of from about 0° C. to about 100° C. thereby causing said cuprous ions to react with

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗