Patents
US 4,863,484 A#11628542 Most CitedExpiredUnited States (USPTO)Utility

Process for producing battery electrodes by electrochemical reduction

9Forward Citations (#11628542 Global)
0.2/yrCitation Velocity (#30322016 Global)
2.09Citation PageRank (#13508436 Global)
27Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Battery electrodes, such as those having nickel hydroxide as electrochemically active material, may be produced according to the invention by reducing the electrodes after normal impregnation processing is completed to remove residual nitrate in the impregnated electrode. The alkali metal hydroxide electrolyte utilized in this reduction may be reused up to 7 to 10 times. The reduced electrodes can be used directly to assemble batteries or may be processed further by a formation and characterization electrolytic cycling of charge and discharge. The alkali metal hydroxide electrolyte utilized in this characterization may be reused up to 22 times.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for reducing an electrode which comprises: immersing a porous metal electrode impregnated with a metal hydroxide in an aqueous alkali metal hydroxide solution having an initial alkali metal hydroxide concentration not greater than about 10 wt. %; and applying an electrical current to said impregnated electrode under conditions effective to cathodically reduce said impregnated electrode, without oxidation thereof, to convert nitrate ions in said electrode to ammonia.

  2. Claim 2Depends on #1

    The method of claim 1 wherein said electrode is reduced at a current density of from about 1 to 20 ma/cm 2 for at least about one hour.

  3. Claim 3Depends on #1

    The method of claim 1, wherein said electrode consists essentially of nickel, cadmium or iron, said metal hydroxide is a hydroxide of nickel, cadmium, silver or iron, and said alkali metal hydroxide is sodi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
US 3,214,355 AProcess for the filling of pores of metallic or metallic coated frames with metallic hydroxides and products thereof196525
US 3,288,643 AProcess for making charged cadmium electrodes196611
US 3,355,325 ABattery plate manufacture19671
US 3,507,699 AProcess for making a nickel electrode197014
US 3,573,101 AMethod for producing a cadmium electrode for nickel cadmium cells197112
US 3,582,403 AProcess for preparing electrodes suitable for alkaline storage batteries19712
US 3,600,226 AMethod for making cadmium electrodes for nickel-cadmium cells19712
US 3,653,967 APositive electrode for use in nickel cadmium cells and the method for producing same and products utilizing same197213
US 3,663,296 AMethod for removal of residual nitrate from negative battery plates19723
US 3,671,320 ABattery plate treatment process19723
US 3,873,368 AProduction of cadmium electrodes19758
US 3,899,351 AFormation of electrodes for alkaline batteries19758
US 3,926,671 AMethod of manufacturing positive nickel hydroxide electrodes197523
US 3,966,494 AImpregnation of electrodes for nickel cadmium batteries19764
US 3,986,893 AMethod for making nickel and cadmium electrodes for batteries19765
US 3,997,364 ANickel activation process19762
US 4,032,697 AMethods of producing electrodes for alkaline batteries19775
US 4,120,757 AMethod of making sintered plaque cadmium electrodes19785
US 4,132,606 AProcess for the manufacture of electrodes19797
US 4,139,423 ASintered negative plate19793
US 4,184,930 AElectrolyzer for basic solutions19807

Non-Patent Literature (4)

  • Andre, Communication Presentation, 3rd Section of French Society of Electricians, Mar. 13, 1941.
  • Falk & Salkind, Alkaline Storage Batteries (Wiley 1969) pp. 79, 125 128, 631 632.
  • Falk & Salkind, Alkaline Storage Batteries (Wiley 1969) pp. 79, 125-128, 631-632.
  • King et al., Proc. Ann. Power Soures Conf., vol. 16, (1962) p. 108.