Al-Mg-Si extrusion alloy and method
Abstract
An extrusion ingot of an Al-Mg-Si alloy, has substantially all the Mg present in the form of particles having an average diameter of at least 0.1 microns of beta'-phase Mg 2 Si in the substantial absence of beta-phase Mg 2 Si. The ingot may be made by casting an ingot of the alloy, homogenising the ingot, cooling the homogenised ingot to a holding temperature of 250° C. to 425° C. at a cooling rate of at least 400° C./h, holding the ingot for 0.25 to 3 hours, and cooling. The ingot has improved extrusion properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of forming an extrusion ingot of an aluminum based Al-Mg-Si alloy, which method comprises the steps of: Casting an ingot of the Al-Mg-Si alloy, Homogenising the ingot, Cooling the homogenised ingot to a temperature of 250° C. to 425° C. at a cooling rate of at least 400° l C./h, Holding the ingot at a holding temperature of from 250° C. to 425° C. for a time to precipitate substantially all the Mg as beta'-phase Mg 2 Si in the substantial absence of beta-phase Mg 2 Si, Cooling the ingot.
- Claim 2Depends on #1
A method as claimed in claim 1, wherein the casting is by means of a short-mold or hot-top direct chill casting process.
- Claim 3Depends on #1
A method as claimed in claim 1, wherein the as-cast ingot has a uniform grain size of 70 to 90 microns and a cell size of 28 to 35 microns over the whole ingot cross section, and further c
Technical Overview & Description