Patents
US 4,859,239 A#17401014 Most CitedExpiredUnited States (USPTO)Utility

Tungsten electrode and method of producing same

6Forward Citations (#17401014 Global)
0.2/yrCitation Velocity (#37951994 Global)
1.73Citation PageRank (#18312129 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An electrode, and method of producing same, including tungsten which has been heated in wet hydrogen at 1050° C. for 5 to 10 minutes, then heated at about 1500° C. for about three hours in a vacuum, and then further heated at about 2800° C. for about 5 minutes in a vacuum.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method of making a tungsten electrode comprising the steps of: providing a basic electrode comprising tungsten; then heating said basic electrode in wet hydrogen at about 1050° C. for about 5 to 10 minutes; then further heating said basic electrode at about 1500° C. for about three hours in a vacuum; and then further heating said basic electrode at about 2800° C. for about 5 minutes in a vacuum.

  2. Claim 2Depends on #1

    The method of claim 1 wherein said further heating at about 1500° C. for about three hours is in a vacuum of about 2 ×10 -7 Torr, and said further heating at about 2800° C. for about five minutes is in a vacuum of about 1 ×10 -6 Torr.

  3. Claim 3Depends on #1

    The method of claim 1 wherein said step of providing said basic electrode comprises mixing tungsten powder and thoria powder as constituents of said basic electrode.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗