Method for obtaining adhesion of urethane sealant to a painted or glass surface
Abstract
A method is disclosed for treatment of a painted or a glass surface providing improved adhesion of a urethane sealant applied thereafter, comprising applying a solution containing p-toluenesulfonic acid, optionally an organofunctional silane, and an appropriate solvent to the painted or the glass surface, the painted surface being cured and devoid of a resin coating, and thereafter contacting the painted or the glass surface with the urethane sealant. A method for joining painted and glass surfaces using a urethane sealant is also disclosed. Compositions useful within these methods are also described.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for treatment of a painted surface of a substrate or a glass surface so as to provide improved adhesion of a urethane sealant applied thereafter, comprising: applying a solution of from about 0.25% to about 5% by weight p-toluenesulfonic acid, about 2.5% by weight organofunctional silane, and from about 92.5% to about 97.25% by weight of a solvent selected from the group consisting of ketones, alcohols and aliphatic esters to the painted or the glass surface, the painted surface being cured and devoid of a resin top coating; and thereafter contacting the painted or glass surface wit
- Claim 2Depends on #1
The method of claim 1 wherein the appropriate solvent is selected from the group consisting of methyl ethyl ketone, isopropanol, and ethyl acetate.
- Claim 3Depends on #1
The method of claim 1 wherein the or
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,959,242 A | Silane grafted poly(vinyl alcohol) film | 1976 | 37 |
| US 4,049,861 A | Abrasion resistant coatings | 1977 | 90 |
| US 4,409,266 A | Process for the shatterproof coating of glass surfaces | 1983 | 44 |