Patents
US 4,846,903 A#75094892 Most CitedExpiredUnited States (USPTO)Utility

Method for producing a grain oriented electrical steel sheet

0Forward Citations (#75094892 Global)
0.0/yrCitation Velocity (#75094892 Global)
0.56Citation PageRank (#75094892 Global)
3Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

In the production of a grain-oriented electrical steel sheet, a slab (1) is current-conduction heated, using the slab (1) as a resistor, under a condition of being on or below an apparent current density (I) of from 40 (A/cm2) to 0.5 P2+100 (A/cm2), P being a pressure of electrodes in kg/cm2.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a grain-oriented electrical steel sheet, wherein an electrical steel slab containing from 0.02 to 0.12% of C, and from 2.0 to 4.0% of Si is heated to a temperature of from 1250° to 1400° C., hot-rolled, cold-rolled once or twice or more with an intermediate annealing, decarburization-annealed and finishing annealed, characterized in that said electrical steel slab itself is used as a current conduction resistor and is heated to said temperature of from 1250° to 1400° C. under a condition of an apparent current density (I) of not less than 40 (A/cm 2 ) and not more than 0

  2. Claim 2Depends on #1

    A method according to claim 1, wherein current is conduc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.