US 4,844,720 A#4831361 Most CitedExpiredUnited States (USPTO)Utility

Process for removal of hydrogen sulfide and hydrogen polysulfide from liquid sulfur

18Forward Citations (#4831361 Global)
0.5/yrCitation Velocity (#17320400 Global)
3.82Citation PageRank (#5132511 Global)
13Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improved method for reducing the hydrogen sulfide and hydrogen polysulfide content of liquid sulfur, wherein, the liquid sulfur is brought into contact with a solid degradation catalyst consisting of alumina or a cobalt-molybdenum impregnated alumina at 250° F. to 320° F., preferably 270°-275° F., in the presence of a gaseous purge stream of air or oxygen enriched air. In addition to exhibiting a many fold increase in rate of reaction relative to the use of either the catalyst without a purge gas or the purge gas alone, the use of an oxygen containing purge gas (such as wet air) in combination with the catalyst (such as alumina) shows a significant improvement, when compared to the use of a dry nitrogen purge in combination with the catalyst under similar conditions, in the kinetics of both the conversion of the polysulfides to sulfide (rate constant of 0.611 for wet air vs. 0.409 for dry nitrogen at 300° F.) and the removal of hydrogen sulfide from liquid sulfur (rate constant of 0.877 in wet air vs. 0.62 for dry nitrogen at 300° F.).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 18.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process for the catalytic degradation of hydrogen polysulfide (H 2 S x ) to hydrogen sulfide (H 2 S) followed by removal of the H 2 S comprising a step in which H 2 S x is converted to H 2 S in liquid sulfur in the presence of a solid catalyst comprising alumina, the improvement which comprises: contacting the liquid sulfur and the catalyst at a temperature in the range of about 250° F. to about 320° F. with a free oxygen containing gas and increasing the rate of the catalytic degradation of H 2 S x to H 2 S and simultaneously purging the H 2 S from the liquid sulfur and increas

  2. Claim 2Independent Claim

    A process of c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "H2 S Removal from Liquid Sulphur", King, Energy Processing Canada, Mar.-Apr. 1974, pp. 40, 42.
  • "The Removal of H2 S Dissolved in Liquid Sulphur", W. J. Rennie, Quarterly Bulletin, vol. IX, No. 4, Jan.-Mar. 1973, pp. 19-23.
  • "The Sulfur-Hydrogen Sulfide System", Wiewiorowski et al., The Journal of Physical Chemistry, vol. 70, No. 1, Jan. 1966, pp. 234-238.
  • H 2 S Removal from Liquid Sulphur , King, Energy Processing Canada, Mar. Apr. 1974, pp. 40, 42.
  • The Removal of H 2 S Dissolved in Liquid Sulphur , W. J. Rennie, Quarterly Bulletin, vol. IX, No. 4, Jan. Mar. 1973, pp. 19 23.