Patents
US 4,842,933 A#4734854 Most CitedExpiredUnited States (USPTO)Utility

Composites with improved fiber-resin interfacial adhesion

18Forward Citations (#4734854 Global)
0.5/yrCitation Velocity (#17313105 Global)
6.29Citation PageRank (#2279744 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The adhesion of fiber reinforcement such as high modulus graphite to a matrix resin such as polycarbonate is greatly enhanced by applying a very thin layer, suitably from 50 Angstroms to below 1000 Angstroms, to the surface of the fiber such as by immersing the fiber in a dilute solution of the matrix resin in a volatile solvent followed by draining to remove excess solution and air drying to remove the solvent. The thin layer wets the fiber surface. The very dilute solution of matrix resin is able to impregnate multifilament fibers and the solution evenly flows onto the surface of the fibers. A thin uniform layer is formed on the surface of the fiber after removal of the solvent. The matrix resin coated fiber is completely wetted by the matrix resin during formation of the composite. Increased adhesion of the resin to the fibers is observed at fracture. At least 65 percent of the surface of the graphite fiber is covered with polycarbonate resin at fracture whereas uncoated fibers have very little matrix resin adhering to their surfaces at fracture and epoxy sized graphite fibers exhibit only slightly higher coverage with matrix resin at fracture. Flexural modulus of the composite

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for improving the the interfacial adhesion of a thermoplastic matrix resin to fiber in a composite comprising the steps of: applying a dilute solution of the matrix resin in volatile solvent to the fibers and drying the fibers to remove the solvent to form a thin layer of a matrix resin having a thickness of from a monolayer to 1000 Angstroms on the fibers before dispersing the matrix-resin coated fibers in a further amount of matrix resin to form a composite, whereby at least 65 percent of the surface of said fibers are coated with the matrix resin at the time of fracture of the comp

  2. Claim 2Depends on #1

    A method according to claim 1 in which the layer has a thickness from 50 Angstroms to 250 Angstroms.

  3. Claim 3Depends on #2

    A method according to claim 2 in which the solution has a concentration 0.1 to 0.2 percent by weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 9,012,533 B2Fiber-reinforced resin composites and methods of making the same20150
US 5,106,680 AAdhesion between carbon fibers and thermoplastic matrix materials in carbon fiber composites by using multifunctional amine and azo compounds as bridging agents199219
FR 2,864,110 A1Device with a hydrophobic and/or lipophobic surface formed of a carpet of nanofibers where the fibres and the surface between them are coated with a polymer film—2
CN 103,261,286 AComposites having distortional resin coated fibers—2
US 2011012163 A1Device having a multilayered structure and method of fabricating thereof—0
US 6,121,169 APorous interfacial coating for fiber reinforced ceramic matrix composites20009
US 2012321836 A1Variable-thickness elecriplast moldable capsule and method of manufacture—11
US 5,077,338 AUsing a solvent for in-situ formation of fibers in an elastomer19914
US 5,001,184 AHigh modulus thermoplastic composites19919
WO 2012/082280 A1Composites having distortional resin coated fibers—2
US 2007110982 A1Device having a hydrophobic and/or lipophobic surface and method of producing one such device—5
US 5,227,199 AProcesses for applying metal oxide coatings from a liquid phase onto multifilament refractory fiber tows199320
US 5,800,874 ATechnique for forming resin-impregnated fiberglass sheets19988
US 5,891,518 ACarbon fiber-coating produced via precursor/solvent solution19997
WO 2005/061129 A1Device having a hydrophobic and/or lipophobic surface and method of producing one such device—2

Non-Patent Literature (5)

  • Cheng, et al., SPE Journal, 26 No. 8 p. 62 (1970).
  • Kardos, et al., Polym. Engn. Sci., 13, 455 (1973).
  • Plueddemann, "Silane Coupling Agents", Plenum Press, N.Y. (1982).
  • Plueddemann, Silane Coupling Agents , Plenum Press, N.Y. (1982).
  • Riess, et al., Proc. 2nd Carbon Fibers Conf., The Plastic Institute, p. 52 (1974).