Thermoplastic molding materials and their preparation
Abstract
A thermoplastic molding material contains, in each case based on the molding material comprising A+B, A from 80 to 60% by weight of a hard matrix composed of polystyrene and B from 20 to 40% by weight of a soft phase which is obtainable by polymerization of styrene in the presence of a linear styrene/butadienne block copolymer which has an ill defined transition, contains from 35 to 45% by weight of styrene and from 65 to 55% by weight of butadiene and has a block polystyrene content of from 25 to 35% by weight, the soft phase being uniformly distributed in the hard matrix and having a particle diameter of less than 0.8 μm. The typical features of the said molding material are that the median particle diameter d 50 (volume average of the soft phase B is from 0.25 to 0.38 μm, the width of the particle size distribution, (d 95 14 d 5 ), is from 0.2 to 0.6 μm, the d 60 value is from 0.26 to 0.40 μm and the d 90 value is from 0.40 to 0.75.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermoplastic molding material consisting essentially of from 80 to 60% by weight of a hard matrix (A) composed of polystyrene and from 20 to 40% by weight of a soft phase (B), the soft phase (B) being uniformly distributed in the hard phase and having a particle diameter of less than 0.8 μm, its median particle diameter d 50 (volume average) being from 0.25 to 0.38 μm, the width of the particle size distribution, (d 95 -d 5 ), being from 0.2 to 0.6 μm, the d 60 value being from 0.26 to 0.40 μm and the d 90 value being from 0.40 to 0.75, said molding material being obtained by batchwis
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗