Consumable welding electrode and method of using same

45Forward Citations (#1150954 Global)
1.2/yrCitation Velocity (#4927947 Global)
3.92Citation PageRank (#4914236 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improved consumable electric arc welding electrode having an outer ferrous metal sheath, such as a low carbon steel sheath, which is formed around a generally concentric core of compressed particulate fill material to be used for depositing an all weld metal of steel in multiple passes with a minimum tensile strength of about 72,000 psi and a minimum elongation of about 22 percent wherein the fill material includes aluminum in an amount greater than about 1.50 percent of the total electrode weight to provide a correlated amount of aluminum in the deposited metal. This improvement involves a particulate fill material producing a combination of nickel and manganese content in the range of 2.5-4.0 percent by weight of the total electrode with the nickel being greater than about 0.5 percent, the manganese being in the range of 0.7-2.0 percent and both the aluminum and the carbon in the fill material being properly controlled whereby the deposited all weld metal, when the sheath and core materials are melted and deposited, has a percentage by weight of aluminum greater than about 1.20 percent and a percentage of carbon by weight of less than about 0.12 percent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 45.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a self-shielding consumable electric arc welding electrode having an outer ferrous metal sheath formed around a generally concentric core of compressed particulate fill material to be used for depositing an all weld metal of steel in multiple passes with a minimum tensile strength of about 72,000 psi and a minimum elongation of about 22%, the improvement comprising: said fill material including aluminum in an amount greater than about 1.50 percent of the total electrode weight, and a combination of nickel and manganese content in the range of 2.5-4.0 percent by weight of the total electrode