US 4,828,631 A#1034311 Most CitedExpiredUnited States (USPTO)Utility

High strength aluminum alloy resistant to exfoliation and method of making

47Forward Citations (#1034311 Global)
1.3/yrCitation Velocity (#4615870 Global)
11.60Citation PageRank (#829403 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method is provided for producing a high strength aluminum alloy characterized by improved resistance to exfoliation. The method comprises providing an aluminum-base alloy comprising 5.9 to 8.2 wt. % zinc, 1.5 to 4.0 wt. % magnesium, 1.5 to 3.0 wt. % copper, less than 0.01 wt. % boron not more than 0.04 wt. % chromium, and 0.5 wt. % maximum other alloying elements such as zirconium, manganese, iron, silicon and titanium, with the balance consisting of aluminum, working the alloy into a product of predetermined shape, solution heat treating the shaped product, quenching, and aging the heat treated and quenched product to a temperature of from above 270 DEG F. for a period of from 6 to 30 hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 47.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a high strength aluminum alloy product characterized by improved resistance to exfoliation which comprises: (a) providing an aluminum-base alloy consisting essentially of 5.9 to 6.9 wt. % zinc, 1.5 to 4.0 wt. % magnesium, 1.5 to 3.0 wt. % copper, less than 0.01 wt. % boron and not more than 0.04 wt. % chromium with the balance comprising aluminum; (b) working the alloy into a shaped product; (c) heat treating the shaped product; (d) quenching the heat treated product; and (e) aging the product at a temperature of from above 265° F. to 290° F. for a period of from

  2. Claim 2Depends on #1

    The method of claim 1 wherein the aging is carried out at a temperature of from 270° F. to 285° F.

  3. Claim 3Depends on #2

    The method of claim 2 wherein said alloy contains 0.08 to 0.15 wt. % zirconium and less than 0.008 w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 47 total)

PatentTitleYearCitations
US 5,785,777 AMethod of making an AA7000 series aluminum wrought product having a modified solution heat treating process for improved exfoliation corrosion resistance199815
US 10,301,710 B2Aluminum alloy that is not sensitive to quenching, as well as method for the production of a semi-finished product20191
US 6,027,582 AThick alZnMgCu alloy products with improved properties200092
US 7,678,205 B2Aluminum alloy products having improved property combinations and method for artificially aging same20106
US 9,353,430 B2Lightweight, crash-sensitive automotive component20160
US 8,206,517 B1Aluminum alloys having improved ballistics and armor protection performance201215
US 2005189044 A1Al-Zn-Mg-Cu alloy with improved damage tolerance-strength combination properties—33
US 8,083,870 B2Aluminum alloy products having improved property combinations and method for artificially aging same20111
US 8,608,876 B2AA7000-series aluminum alloy products and a method of manufacturing thereof20137
US 8,840,737 B2Aluminum alloy products having improved property combinations and method for artificially aging same20142
US 5,221,377 AAluminum alloy product having improved combinations of properties1993126
US 6,726,878 B1High strength aluminum based alloy and the article made thereof20045
US 7,883,591 B2High-strength, high toughness Al-Zn alloy product and method for producing such product20112
US 2007125460 A1HIGH CRASHWORTHINESS Al-Si-Mg ALLOY AND METHODS FOR PRODUCING AUTOMOTIVE CASTING—21
US 2005257865 A1Aluminum alloy products having improved property combinations and method for artificially aging same—2

References Cited — Backward Prior Art (2)