Abstract

PCT No. PCT/SE86/00070 Sec. 371 Date Oct. 2, 1986 Sec. 102(e) Date Oct. 2, 1986 PCT Filed Feb. 19, 1986 PCT Pub. No. WO86/04841 PCT Pub. Date Aug. 28, 1986.Method in producing a molding of an iron alloy, wherein the molding is produced by hot isostat pressing of a prealloyed powder comprising 0.5 to 2.8% coal by weight, 24 to 35% chromium by weight, from effective amount to 2% silicon by weight, from effective amount to 1.5% manganese by weight, 0 to 2.3% nickel weight, and 0 to 3.0% molybdenum by weight, and the residue iron.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Method in producing a shaped molding of an iron alloy, characterized in that the molding is produced by hot isostatic pressing of a prealloyed powder comprising 0.5 to 2.8 % coal by weight, 24 to 35 % chromium by weight, from effective amount to 2 % silicon by weight, from effective amount to 1.5 % manganese by weight, 0 to 2.3 % nickel by weight, and 0 to 3.0 % molybdenum by weight, and the residue iron.

  2. Claim 2Depends on #1

    Method as claimed in claim 1, characterized in that the hot isostatic pressing is performed at a pressure ranging between 100 and 150 MPa, and at a temperature ranging between 1230° and 1270° C.

  3. Claim 3Depends on #2

    Method as claimed in claim 2, characterized in that the molding produced after pressing is allowed to cool to room temperature in the press and then, after removal from the press, is exposed to heat treatment at a temperatur

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • E. Houdremont & R. Wasmuht: Non Rusting & Heat Resisting 34% Chromium Alloy Cast Irons Metals & Alloys, Feb. 1933, s 13 17.
  • E. Houdremont & R. Wasmuht: Non-Rusting & Heat Resisting 34% Chromium Alloy Cast Irons Metals & Alloys, Feb. 1933, s 13-17.
  • MNC Handbok nr 3, 1978, Gjutlegeringar, s 106.
  • S. Friborg: HIP to Near Net Shape, Scand J. Metallurgy 11(1982), s 223 225.
  • S. Friborg: HIP to Near Net Shape, Scand J. Metallurgy 11(1982), s 223-225.