Abstract
In a process for preparing a spherical copper fine powder having an average grain size ranging from 0.1 μm to a few μm, by use of chemical vapor deposition of cuprous chloride vapor with a reducing gas, the vapor deposition zone is maintained at a temperature ranging 900° C. to less than 1,150° C. and the generated particles are quenched subsequently. The generated powder is utilized as a conductive powder which is the main component of a conductive paste.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 16.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process of making fine, spherical copper powder comprising the steps of introducing a gaseous mixture of a reducible copper compound and an inert gas into a vapor deposition zone to contact a reducing gas; maintaining the zone at a temperature ranging from 900° C. to less than 1150° C. to generate fine, spherical copper particles; quenching the generated particles.
- Claim 2Depends on #1
A process claimed in claim 1 which further comprises determining a combination of an evaporation temperature of cuprous chloride and a flow rate of the inert gas for obtaining an average grain size ranging from 0.1 μm to a few μm .
- Claim 3Depends on #1
A process claimed in claim 1 which comprises quenching the generated particles at a rate of more than 1500 deg/sec, whereby the particles remain as a generated state of spherical shape.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (2)
- Funtai Kogaku Kaishi, vol. 21, pp. 759 767, 1984.
- Funtai Kogaku-Kaishi, vol. 21, pp. 759-767, 1984.