Method for the preparation of high surface area amorphous transition metal chalcogenides
Abstract
A process for the direct synthesis of high surface area amorphous chalcogenides of transition metals of Group IV, V, VI and VII elements, comprising the steps of: (1) forming a mixture of: (a) a halide of a said transition metal having the formula MY n where Y is chlorine, bromine, flurorine, or iodine, and n is 3, 4, 5 or 6, and (b) a source of chalcogen selected from compounds having the formula (R) 3 Si--X--Si(R) 3 wherein R is alkyl having from 1-4 carbon atoms and X is sulfur, selenium or tellurium, (2) reacting said mixture at a temperature of -77° C. to +160° C.; (3) separating the transition metal chalcogenide from the reaction mixture; and (4) washing said chalcogenide with an inert solvent to remove unreacted materials and the byproducts of the reaction. The high surface area amorphous chalcogenides prepared according to the covalent exchange process of the invention are advantageously used in primary or secondary batteries, particularly lithium cells. They are of amorphous chemical structure as shown by X-ray, Raman and infrared analysis. Their small crystal size, high surface area, and freedom from oxygen and water contamination, make them high activity, rechargeable ca
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for the direct synthesis of X-ray amorphous sulfides or selenides of molybdenum comprising the steps of: (1) forming a mixture of: (a) a halide of molybdenum having the formula MoY n where Y is chlorine, bromine, fluorine of iodine and n is 4,5 or 6, and (b) a source of sulfur or selenium selected from: (i) hexamethyl disilathiane or (ii) hexamethyl disilaselenane, (2) reacting the mixture formed in (1) at a temperature of from -77° C. to +160° C.; and (3) separating the molybdenum sulfide or selenide formed in step (2).
- Claim 2Depends on #1
The process of claim 1 wherein a stochiometric excess of hexamethyl disilathiane or hexamethyl disilaselenane is employed.
- Claim 3Depends on #1
A process as recited in claim 1 wherein the reaction mixture is formed in a nonreactive solvent selected from the group consisting of tetrahydrofu
Technical Overview & Description