Protective tip for a titanium blade and a method of brazing such a tip
Abstract
A protective tip (5) for a titanium steam-turbine blade (1), comprises 28% to 40% TiC, 12% to 26% Cr+Co, 1% to 6% Mo, 3% to 8% Ni 0.3% to 1.5% Cu and a balance of Fe. The tip (5) is brazed to the blade (1) by interposing a copper-based strip (6) having a thickness lying between 7/100 mm and 15/100 mm therebetween, then raising the temperature of the blade (1) and its tip (5) to between 900° C. and 950° C. in a vacuum or inert atmosphere oven. This temperature is maintained for a period of between thirty minutes and seventy-five minutes, and the oven is allowed to cool to ambient temperature. Optimal brazing also serves to harden the tip (5) possesses very good resistance to abrasion by water droplets.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 37.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A protective tip for a titanium turbine blade, said tip comprising the following constituents: TiC: 28% to 40% Cr+Co: 12% to 26% Mo: 1% to 6% Ni: 3% to 8% Cu: 0.3% to 1.5% Fe: balance
- Claim 2Depends on #1
A method of brazing a tip according to claim 1 onto a titanium blade, the method comprising the following steps: the tip is placed on the blade and a copper-based strip having a thickness lying between 7/100 mm and 15/100 mm is interposed therebetween; the temperature of the blade and its tip is raised to between 900° C. and 950° C. in a vacuum or inert atmosphere oven and this temperature is maintained for a period of between thirty minutes and seventy-five minutes; and the temperature is cooled to ambient.
- Claim 3Depends on #2
A method according to claim 2, wherein after cooling down to ambient, the temperature is raised to 450° C. to 50