Patents
US 4,790,902 A#614784 Most CitedExpiredUnited States (USPTO)Utility

Method of producing conductor circuit boards

62Forward Citations (#614784 Global)
1.6/yrCitation Velocity (#3017136 Global)
21.33Citation PageRank (#300035 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A thin metal layer with a thickness of 1 to 5 μ is formed electrolytically (S2) on an electrically conductive single-plate substrate having a predetermined roughness, a resist mask is formed (S3) on the surface of the thin metal layer, and a conductor circuit is then electroformed thereon (S4) using copper. After the surface of the conductor circuit is roughened (S5), the conductor circuit, along with the single plate and the interposed thin metal layer, is stacked on an insulating substrate for lamination, and the individual layers are adhered integrally to one another by the application of heat and pressure (S7). Then, the single plate only is peeled off (S8), and the exposed thin metal layer is removed by etching (S9). The thin metal layer and the conductor circuit are electroplated under high-speed conditions including a solution contact speed of 2.6 to 20 m/sec and a current density of 0.15 to 4.0 A/cm 2 , so that a required adhesion force can be obtained between the thin metal layer and the resist mask, and the conductor circuit can be made as flexible as rolled annealed copper. Thus, very thin, high-density conductor circuits can be produced which, having a thickness of 10 μ

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 62.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing conductor circuit boards comprising steps of: forming a thin metal layer with a thickness of 1 to 5 μm on a planar, electrically conductive substrate with a surface roughness of 0.08 to 0.23 μm, for use as a cathode, by spacing said cathode and a planar anode at an interelectrode distance of 3 to 30 mm from each other, and compulsorily supplying an electrolytic solution to said electrodes so that said electrolytic solution comes into contact with said electrodes at a solution contact speed of 2.6 to 20.0 m/sec, thereby electroplating said electrodes under the condition of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗