Process for the production of heat resistant thermoplastic copolymer
Abstract
A process for the production of a thermoplastic copolymer having excellent heat distortion resistance is disclosed. The process includes heat-treating a raw copolymer comprising a vinyl monomer unit including methacrylic and/or acrylic acid units in the presence of a specific ring-closing promoter selected from basic compounds, whereby the methacrylic and/or acrylic acid unit is converted into six-membered cyclic anhydride unit. The copolymer has excellent heat distortion resistance, transparency, mechanical properties and processability, and can produce a formed product without splash on the surface. The copolymer is useful for the production of various parts, such as automobile parts, electrical parts, industrial parts, and miscellaneous goods.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 16.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for the production of a copolymer, which comprises heat-treating a raw copolymer comprising units of a vinyl monomer and 5 to 50% by weight of a methacrylic and/or acrylic acid unit in the presence of 0.01 to 0.5% by weight of a basic compound, thereby converting the methacrylic and/or acrylic acid unit into a six-membered cyclic anhydride unit, wherein the vinyl monomer is a member selected from the group consisting of methacrylic esters, acrylic esters and aromatic vinyl compounds, and the basic compound is a member selected from the group consisting of alkali metal hydroxides or c
- Claim 2Depends on #1
The process according to claim 1, wherein the heat treatment is carried out at a temperature of 150° to 350° C.