Abstract
Metal leads are prepared for solder dipping by first exposing the leads to a fifty percent solution of sulfuric acid. The leads are then rinsed using city water and exposed to solution consisting of fifty percent sulfuric acid, twenty-five percent nitric acid and twenty-five percent deionized water. The leads are then rinsed sequentially in city water and deionized water. Finally, excess water is removed from the leads.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of removing oxides from the surface of the metal leads that extend from a packaged semiconductor integrated circuit device, the method comprising the steps of: a. exposing the leads to a fifty percent solution of sulfuric acid; b. rinsing the leads with city water; c. exposing the leads to a solution consisting of about fifty percent sulfuric acid, twenty-five percent nitric acid and twenty-five percent deionized water; d. sequentially rinsing the leads in city water and deionized water; and e. removing water from the leads.
- Claim 2Depends on #1
A method as in claim 1 wherein the sulfuric acid solution utilized in step (a) of claim 1 is at about 150° F.
- Claim 3Depends on #1
A method as in claim 1 wherein the deionized water is 2 M Ohm deionized water.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,083,848 A | Removing solder from integrated circuits for failure analysis | 2000 | 5 |
| US 4,963,233 A | Glass conditioning for ceramic package plating | 1990 | 2 |