Patents
US 4,772,571 A#599496 Most CitedExpiredUnited States (USPTO)Utility

Process of self aligned nitridation of TiSi2 to form TiN/TiSi2 contact

63Forward Citations (#599496 Global)
1.7/yrCitation Velocity (#2968873 Global)
12.05Citation PageRank (#779182 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In order to prevent diffusion of silicon from under a titanium disilicide interconnect (1) and into an overlying aluminium layer (6), the disilicide is selectively nitrided by annealing in nitrogen at the points where interconnection between the disilicide and aluminium is required via holes (4) in a silicon dioxide layer (3). The titanium nitrode contacts (5) thus formed in a truly self-aligned manner provide a good barrier to silicon diffusion while having an acceptable low resistivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 63.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device including the steps of forming a titanium disilicide element on a semiconductor wafer, providing an electrically insulating layer over the wafer, exposing a region of the titanium disilicide element via a hole in the electrically insulating layer, annealing the wafer in nitrogen whereby to form titanium nitride at the exposed titanium disilicide region, metallising the wafer, and patterning the metallisation to form a metal element, the titanium disilicide element being in electrical contact with the metal element via the titanium nitride, which

  2. Claim 2Depends on #1

    A method as claimed in claim 1 wherein the insulating layer is of silicon dioxide.

  3. Claim 3Depends on #1

    A method as claimed in claim 1 wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 63 total)

PatentTitleYearCitations
US 7,834,338 B2Memory cell comprising nickel-cobalt oxide switching element20104
US 7,812,404 B2Nonvolatile memory cell comprising a diode and a resistance-switching material201027
US 5,658,828 AMethod for forming an aluminum contact through an insulating layer199732
US 8,233,308 B2Memory cell that employs a selectively deposited reversible resistance-switching element and methods of forming the same20126
US 5,371,041 AMethod for forming a contact/VIA199445
US 5,930,673 AMethod for forming a metal contact19994
US 6,271,137 B1Method of producing an aluminum stacked contact/via for multilayer200116
US 8,913,417 B2Memory cell that employs a selectively deposited reversible resistance-switching element and methods of forming the same20141
US 8,816,315 B2Memory cell that employs a selectively grown reversible resistance-switching element and methods of forming the same20140
US 8,507,315 B2Memory cell that employs a selectively grown reversible resistance-switching element and methods of forming the same20130
US 9,761,461 B2Systems and methods for fabricating a polycrystaline semiconductor resistor on a semiconductor substrate20170
US 8,173,486 B2Memory cell that employs a selectively grown reversible resistance-switching element and methods of forming the same20120
US 2009001343 A1Memory cell that employs a selectively deposited reversible resistance-switching element and methods of forming the same—63
US 5,760,475 ARefractory metal-titanium nitride conductive structures199854
US 4,931,411 AIntegrated circuit process with TiN-gate transistor199097

Non-Patent Literature (5)

  • C. Y. Ting and M. Wittmer, Thin Solid Films, 96 (1982), pp. 327 345.
  • C. Y. Ting and M. Wittmer, Thin Solid Films, 96 (1982), pp. 327-345.
  • C. Y. Ting, J. Vac. Sci. Technol., 21 (1), May/Jun. 1982, pp. 14 18.
  • C. Y. Ting, J. Vac. Sci. Technol., 21 (1), May/Jun. 1982, pp. 14-18.
  • M. A. Nicollet, Thin Solid Films, 52 (1978), pp. 415 445.