Patents
US 4,770,720 A#2059263 Most CitedExpiredUnited States (USPTO)Utility

Method for producing a grain-oriented electrical steel sheet having a low watt-loss

32Forward Citations (#2059263 Global)
0.8/yrCitation Velocity (#8633590 Global)
4.11Citation PageRank (#4554148 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

PCT No. PCT/JP85/00627 Sec. 371 Date Sep. 5, 1986 Sec. 102(e) Date Sep. 5, 1986 PCT Filed Nov. 11, 1985 PCT Pub. No. WO86/02950 PCT Pub. Date May 22, 1986.Grooves are formed on a finish-annealed electrical steel sheet by applying a mean load of from 90 to 220 kg/mm2 to the steel sheet, which is then heat treated at a temperature of 750 DEG C. or higher, and thereby fine crystal grains are generated at the strain-introduced sites of the steel sheet. The fine crystal grain reduces the watt-loss value. Such a watt-loss improving effect is not impaired even by stress-relief annealing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 32.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a grain-oriented electrical steel sheet having a low watt-loss, wherein grooves are formed on an electrical steel sheet that has been final-texture annealed, or final-texture annealed and then subjected to an insulation-coating-treatment, by locally loading at a mean load of from 90 to 220 kg/mm 2 at an angle in a range of from a right angle to 45° to a rolling direction, and then said steel sheet is heat-treated at a temperature of 750° C. or higher.

  2. Claim 2Depends on #1

    A method according to claim 1, wherein said grooves are so formed as to be spaced at an interval of from 1 to 20 mm in the rolling direction, have a width of from 10 to 300 μm, and have a depth in the steel body of 5 μm or more.

  3. Claim 3Depends on #2

    A method according to claim 2, wherein said grooves have an interval therebetween of from 2.5 to 10 mm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 32 total)

PatentTitleYearCitations
US 5,483,811 ASegmented anvil roller for refining the domain structure of electrical steels19969
US 6,261,702 B1Embossed rolled steel and embossing roll and method for making the same200115
US 10,131,018 B2Grain-oriented magnetic steel sheet and method of producing the same20182
US 8,202,374 B2Method of treating steel for grain-oriented electrical steel sheet and method of manufacturing grain-oriented electrical steel sheet20122
US 8,034,196 B2Low core loss grain-oriented electrical steel plate and method of manufacturing the same20114
US 11,512,360 B2Grain-oriented electrical steel sheet with excellent magnetic characteristics20220
US 12,065,713 B2Grain-oriented electrical steel sheet20240
US 5,085,411 AApparatus for processing grain-oriented electrical steel strip19924
US 5,588,321 ASegmented scribing roller for refining the domain structure of electrical steels by local mechanical deformation19965
US 8,784,995 B2Grain oriented electrical steel sheet and method for manufacturing the same20144
US 5,408,856 AApparatus for domain refining electrical steels by local mechanical deformation with multiple scribing rolls19950
EP 0,378,131 A3A method of manufacturing a grain-oriented electrical steel strip—0
US 9,406,437 B2Grain oriented electrical steel sheet and method for manufacturing the same20166
US 11,898,215 B2Grain-oriented electrical steel sheet and method for manufacturing the same20240
US 8,657,968 B2Grain-oriented electrical steel sheet and method of manufacturing the same20142