Thermoplastic elastomers
Abstract
Thermoplastic elastomers made of 48 to 88% by weight of ethylene-propylene-diene-rubber (EPDM), 10 to 50% by weight of polypropylene (PP) and 2 to 20% by weight of a third polymer and 5 to 60% by weight of softening oil, based on the total of EPDM, PP and the third polymer, and optionally further conventional constituents, have the advantage that the softening oil does not exude.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Thermoplastic elastomer containing a polymer mixture consisting essentially of (i) 48-88% by weight of ethylene-propylene-diene-rubber, 10-50% by weight of polypropylene and 2-20% by weight of a block-copolymer made of at least two blocks A and B, whereby block A is polystyrene and block B is polybutadiene or polyisoprene, and the polymer of block B is at least partially hydrogenated, and (ii) 5-60% by weight of a plasticizing oil with the percentages of component (ii) being based on the total of the components of (i).
- Claim 2Depends on #1
Thermoplastic elastomers according to claim 1 wherein component (i) has 15-30% ethylene-propylene-diene-rubber, 15-30% polypropylene and 3-10% block-copolymer and component (ii) has an amount of 20-40%.
- Claim 3Depends on #1
Thermoplastic elastomers according to claim 1, in which the ethylene-propylene-diene-rubb
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (2)
- Holden et al., "Block & Graft Copolymerization", Chapter 6, pp. 133 & 171.
- Holden et al., Block & Graft Copolymerization , Chapter 6, pp. 133 & 171.