Carburization/oxidation resistant worked alloy
Abstract
An iron-nickel-chromium-aluminum alloy containing about 30 to 40% nickel, about 15 to less than 19% chromium, about 2 to 4% aluminum, carbon in an amount of at least 0.05% and up to 0.2%, about 0.2 to 0.8% titanium, from 1.5 to 4% molybdenum, up to 0.1% boron, up to 0.5% zirconium, up to about 5% cobalt and the balance iron. Alloy is characterized by (i) carburization resistance and (ii) stress-rupture strength which is desirable for ethylene pyrolysis tubing, (iii) highly oxidation resistant, (iv) cold workable such that mill product forms can be readily produced without deleterious cracking, (vi) ductile, (vii) structurally stable, i.e., will resist forming detrimental quantities of undesirable phases such as sigma, and (viii) weldable.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A highly (i) oxidation and (ii) carburization resistant alloy at temperatures as high as 1800°-2000° F. and further characterized by (iii) good stress-rupture properties at such temperatures while also manifesting (iv) hot and (v) cold workability together with good (v) ductility, (vi) structural stability and (vii) weldability, said alloy in the worked condition having an average grain size of from ASTM 00 to about ASTM 2 and consisting essentially of 32 to 38% nickel, about 15 to less than 19% chromium, about 2 to 4% aluminum, at least 0.07 to 0.15% carbon, from 1.5 to 3.5% molybdenum, about
- Claim 2Depends on #1
The alloy of claim 1 containing 2.5 to 3.5% aluminum and 2 to 3.5% molybdenum.
- Claim 3Depends on #1
The alloy of claim 1 conta
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (5)
- A. Schnaas and H. J. Grabke, "High Temperature Corrosion and Creep of Ni-Cr-Fe Alloys in Carburizing and Oxidizing Environments", Nov. 5, 1978.
- A. Schnaas and H. J. Grabke, High Temperature Corrosion and Creep of Ni Cr Fe Alloys in Carburizing and Oxidizing Environments , Nov. 5, 1978.
- D. E. Hendrix and Malcolm W. Clark, P.E., "Contributing Factors to the Unusual Creep Growth of Furnace Tubing in Ethylene Pyrolysis Service", Paper No. 21, Corrosion 85, pp. 21/1-21/11--Mar. 25-29, 1985, Sheraton Hotel.
- D. E. Hendrix and Malcolm W. Clark, P.E., Contributing Factors to the Unusual Creep Growth of Furnace Tubing in Ethylene Pyrolysis Service , Paper No. 21, Corrosion 85, pp. 21/1 21/11 Mar. 25 29, 1985, Sheraton Hotel.
- J. J. Moran and J. W. Schultz, "The High Temperature Corrosion Resistance of Iron-Nickel-Chromium Alloy Containing Some Aluminum", Apr. 3, 1967.