Method of forming silicon nitride coating
Abstract
A silicon nitride coating is deposited on the inside surface of a crucible by pyrolysis. Reactive gases are fed through a tube into the crucible. The crucible is rotated during deposition and the crucible walls are maintained at a temperature of at least about 1250° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 45.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
The method of depositing a silicon nitride coating on the inside surface of a crucible comprising the steps of: disposing the crucible inside a reaction chamber; positioning a closed end tube axially within the crucible, the tube having a plurality of peripheral holes at the lower end thereof; introducing reactive gases into the tube and out through the peripheral holes to the inside surface of the crucible where the gases react to produce and deposit silicon nitride coating; rotating the crucible during deposition to obtain uniformity of coating; maintaining crucible temperature during deposi
- Claim 2Depends on #1
The method of claim 1 wherein the reactive gases comprise ammonia and silicon tetrachloride.
- Claim 3Independent Claim
The method
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗