Abrasive material, especially for turbine blade tips

69Forward Citations (#504414 Global)
1.8/yrCitation Velocity (#2472942 Global)
9.81Citation PageRank (#1095101 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An abrasive material comprised of a metal matrix and evenly distributed ceramic particulates, is made by mixing powder metal with the ceramic powder and heating to a temperature sufficient to melt most, but not all of the powder. In this way the ceramic does not float to the top of the material, yet a dense material is obtained. A nickel superalloy matrix will have at least some remnants of the original powder metal structure, typically some equiaxed grains, along with a fine dendritic structure, thereby imparting desirable high temperature strength when the abrasive material is applied to the tips of blades of gas turbine engines. Preferred matrices have a relatively wide liquidus-solidus temperature range, contain a melting point depressant, and a reactive metal to promote adhesion to the ceramic.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 69.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method of making an abrasive material comprised of evenly dispersed ceramic particulates surrounded by a fused matrix of metal having a density greater than the density of the ceramic material, characterized by mixing metal particulate with ceramic particulate, heating the mixture to a temperature sufficient to cause partial melting of the metal so that it fuses into a dense matrix when cooled, but insufficient to cause the ceramic particulate to substantially float in the metal matrix.

  2. Claim 2Depends on #1

    The method of claim 1 characterized by producing a metallurgical structure which is a combination of equiaxed grains and fine dendrites.

  3. Claim 3Depends on #1

    The method of claim 1 characterized by the metal being a superalloy based on nickel, cobalt, iron or mixtures thereof.