Ore pelletization
Abstract
Finely divided mineral ore is pelletized using a soluble synthetic polymer. Preferably the polymer is in the form of beads made by reverse phase polymerization and all having a size of below 300 μm. When the ore gives a pH in water of below 8 the soluble polymer is preferably cationic.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 19.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process in which mineral ore pellets are made by adding binder comprising organic polymer to particulate iron ore having substantially all particles below 250 μm and stirring in the presence of 5 to 15% by weight water (based on total mix) to form a substantially homogeneous moist mixture and pelleting the moist mixture, and in which the binder comprises about 0.002% to about 0.5% by weight, based on total mix, of a water soluble synthetic polymer and that is added to the ore as dry, free flowing beads that are substantially all above 20 μm and below 300 μm and that are made by reverse phase
- Claim 2Depends on #1
A process according to claim 1 in which the binder gives a surface tension of above 70 dynes/cm at a concentration in water at 20° C. of 0.075%.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗