Patents
US 4,717,455 A#11187768 Most CitedExpiredUnited States (USPTO)Utility

Process for manufacturing a microfilter

9Forward Citations (#11187768 Global)
0.2/yrCitation Velocity (#30270429 Global)
2.79Citation PageRank (#8528257 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process for manufacturing a microfilter is such that a foil having an aluminum content of at least 99.95% and thickness 20-250 μm is given a recrystallizing anneal, is etched in an electrolyte in stages at constant current density in the range 0.01 to 2 kA/m 2 , and the surface given a stabilizing after treatment to prevent hydration reactions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Process for manufacturing a microfilter from a recrystallized aluminum foil using electrolytic etching, which comprises: providing a 20 to 250 μm thick aluminum foil of at least 99.95% purity, subjecting said foil to a recrystallizing anneal, etching in an electrolyte in at least one step of constant current density in the range of 0.1 to 2.0 kA/m 2 to form an aluminum foil having through-flow pores suitable for use as a microfilter, and stabilizing the surface of the resultant product to prevent a hydration reaction.

  2. Claim 2Depends on #1

    A process according to claim 1 wherein an aluminum foil of 20-120 μm thickness is employed and etching takes place on only one side.

  3. Claim 3Depends on #1

    A process according to claim 1 wherein the etched pores are made narrower by anodizing in a barrier layer electrolyte prior to the stabilizing after treatment.