Method for thermal treatment of alloy for heat transfer pipes
Abstract
An alloy for heat transfer pipes excellent in an alkali stress corrosion cracking resistance which is obtained by heating and retaining said alloy at a temperature within the range of a temperature (T°C.), at which a carbide in said alloy is thoroughly solubilized, to T+100° C. for 1 minute or more; cooling it once to a level of 200° C. or less; and carrying out a thermal treatment under conditions within a hatched range Z in FIG. 2, said alloy comprising: in terms of % by weight, 0.15% or less of C; 1.0% or less of Si; 1.0% or less of Mn; 25 to 35% of Cr; 40 to 70% of Ni; 0.5% or less of Al; 0.01 to 1.0% of Ti; 0.5 to 5.0%, in all, of one or more of Mo, W and V; 0.30% or less of P; 0.020% or less of S; and the residue of Fe and impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing an alloy for heat transfer pipes with excellent alkali stress corrosion cracking resistance, said alloy consisting essentially of, in percent by weight: not more than 0.15% C, not more than 1.0% Si, not more than 1.0% Mn, 25to 35% Cr, 40 to 70% Ni, not more than 0.5% Al, 0.01 to 1.0% Ti; 0.5 to 5.0% of a metal selected from the group consisting of Mo, W van V and mixtures thereof, not more than 0.030% P, not more than 0.020% S and the balance Fe and impurities, which process comprises (1) maintaining a mixture containing the metallic components at
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗