Process for reducing the concentration of heavy metals in geothermal brine sludge
Abstract
A process is provided for reducing the total concentration of heavy metals, notably lead, copper and zinc, naturally occurring in silica-rich sludge precipitated from geothermal brine in a brine handling system such as a geothermal brine electric generating plant. The process includes washing the sludge with hot water to displace any brine entrapped in the sludge, dewatering the washed sludge and leaching the silicious solids residue with hydrochloric acid having a concentration of between about 2 and about 9 weight percent and an acid-to-sludge weight ratio between about 0.10 and about 0.33. The acid-sludge mixture is heated to a temperature of at least about 50° and the leaching time is at least about one hour. The leaching solution is separated from the leached sludge and the solids residue are washed with water. Preferably the water used in both washing steps is condensate of steam derived from the geothermal brine. Effluent from the process is preferably combined with the brine for reinjection.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 24.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for reducing the total concentration of heavy metal in silica sludge precipitated from a flow of geothermal brine, the process comprising: (a) washing the silica sludge with hot water so as to replace with said water geothermal brine which is entrapped in said sludge; (b) contacting the washed sludge with a hydrochloric acid solution having a weight ratio of hydrochloric acid relative to said washed sludge causing the pH of the acid-sludge mixture to be less than about 1; (c) separating a silicious solids residue from the hydrochloric acid solution, and (d) washing the siliciou
- Claim 2Depends on #1
The process as claimed in claim 1 wherein the washed sludge is contacted with hydrochloric acid solution for at least about one hour. 3