Patents
US 4,703,884 A#2417292 Most CitedExpiredUnited States (USPTO)Utility

Steel bonded dense silicon nitride compositions and method for their fabrication

29Forward Citations (#2417292 Global)
0.7/yrCitation Velocity (#10320268 Global)
3.87Citation PageRank (#5033577 Global)
21Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A two-stage bonding technique for bonding high density silicon nitride and other ceramic materials to stainless steel and other hard metals, and multilayered ceramic-metal composites prepared by the technique are disclosed. The technique involves initially slurry coating a surface of the ceramic material at about 1500 DEG C. in a vacuum with a refractory material and the stainless steel is then pressure bonded to the metallic coated surface by brazing it with nickel-copper-silver or nickel-copper-manganese alloys at a temperature in the range of about 850 DEG to 950 DEG C. in a vacuum. The two-stage bonding technique minimizes the temperature-expansion mismatch between the dissimilar materials.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 29.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a multilayered ceramic-metal composite comprising: (a) polishing a surface of a dense ceramic material to enhance wetting and reaction with molten reactive material; (b) applying a thin slurry coating of a fine powder mixture of a refractory material comprising a mixture of powdered nickel and molybdenum silicide and bonding it to said surface of said ceramic material; (c) grinding said layer of refractory material to uniform thickness; (d) brazing a surface of said layer of refractory material with a metal alloy at elevated temperatures; and (e) pressure bondin

  2. Claim 2Depends on #1

    The method of claim 1, wherein said refractory material is melted on to said surface of said ceramic material at a temperature of about 1500° C. in vacuum.

  3. Claim 3Independent Claim

    The method

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Ceramic Age, "High Temperature Metal Ceramic Seals", p. 15, Apr. 1954.
  • Ceramic Age, High Temperature Metal Ceramic Seals , p. 15, Apr. 1954.
  • Metals Handbook, 8th edition, vol. 1, p. 30, 1961.
  • R. L. Landingham and T. E. Shell, "Bonding Dense Si3 N4 Components to Steel for Elevated-Temperature Cycling Applications", UCRL-90188, Lawrence Livermore National Laboratory, Livermore, California, 94550, Draft, 9/20/84.
  • R. L. Landingham and T. E. Shell, Abstract, 1/6/83.