Method for the multi-stage fibre cables and the apparatus required for it
Abstract
An improved method for the after-treatment of washed and dried fibre cable having a minimum mass of 250 ktex by crimping, fixing, cooling and optionally cutting or tearing is achieved in that the band width of the cable issuing from the drier with a covering density of at most 5 ktex/cm is reduced by at least 50% of the original band width with a corresponding increase in the packing density, is crimped in a stuffer box crimping means at a stuffer box pressure of from 4 to 10 N/cm and a stuffer box temperature of from 80° to 95° C., the crimping is fixed in or immediately after the stuffer box, the cable is deposited on the surface of an air-permeable conveyor belt, air is blown or sucked there through fibre package or conveyor belt and the cable is then optionally supplied to a tearing converter or a cutting machine.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a method for the after-treatment of washed and dried fibre cables having a minimum mass of 250 ktex by crimping, fixing, cooling and optionally cutting or tearing, the improvement wherein the band width of the dried cable with a covering density of at most 5 ktex/cm is reduced by at least 50% of the original band width by dividing the original cable into at least two individual bands and packing the bands one over the other to obtain a corresponding increase in the packing density is crimped in a stuffer box crimping means at a stuffer box pressure of from 1.5 to 6N/cm 2 and a stuffer box
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗