Patents
US 4,701,428 A#437963 Most CitedExpiredUnited States (USPTO)Utility

Catalyst of silicon and titanium having high mechanical strength and a process for its preparation.

74Forward Citations (#437963 Global)
1.9/yrCitation Velocity (#2285391 Global)
11.93Citation PageRank (#791862 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention discloses a catalyst on the basis of silicon and titanium having the form of microspheres and constituted by oligomeric silica and by titanium-silicalite crystals having an oligomeric silica/titanium-silicalite molar ratio comprised within the range of from 0.05 to 0.11, wherein the crystals of titanium-silicalite are encaged by means of Si-O-Si bridges.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 74.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A silicon and titanium catalyst, in form of microspheres, comprising oligomeric silica and crystals of titanium-silicalite with an oligomeric silica/titanium-silicalite molar ratio in the range of from 0.05 to 0.11, wherein said crystals of titanium-silicalite are encaged with each other by means of Si-O-Si bridges.

  2. Claim 2Depends on #1

    Catalyst according to claim 1, wherein said microspheres have a diameter comprised within the range of from 5 to 1000 μm.

  3. Claim 3Depends on #1

    A process for the preparation of the catalyst as defined in claim 1 by preparing an aqueous solution of silica and tetraalkyl-ammonium hydroxide by hydrolyzing in the liquid phase a tetraalkyl-orthosilicate in an aqueous solution of tetraalkyl-ammonium hydroxide at a temperature in the range of from room temperature to 200° C. and at a time of from 0.2 to 10 hours; dispersing crystals

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗