Patents
US 4,699,657 A#6984685 Most CitedExpiredUnited States (USPTO)Utility

Manufacture of fine grain metal powder billets and composites

14Forward Citations (#6984685 Global)
0.4/yrCitation Velocity (#21826498 Global)
2.36Citation PageRank (#11174895 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Very fine grain metal billets are produced by loading alloy metal powder of desired composition into a metal extrusion container in successive layers of two or four inches deep. Each layer after loading is compacted by a high energy rate forming ram so as to introduce energy on the order of 3×10 6 psi per layer and at least 18×10 6 psi total. An inner plate is then loosely placed on the compacted powder. On top of the inner plate is placed a cover plate which is welded to the container. The filled container is then heated in a furnace to an extrusion temperature below the melting point of the alloy and is extruded in an extrusion press having a ratio of about 3:1 with a force of about 3,000 tons. The inner plate does not move at the same rate as the container and in effect is partially extruded against the powder so as to raise the density of the extruded billet to substantially 100% of its theoretical density. The energy stored in the compacted powder is released by the heating and the extrusion causing multiple dislocations of the grain within a given particle and resulting in a very fine grain size, as small as 25 on the Snyder-Graff intercept scale. If desired the powder may be

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    The method of producing dense billets of metal powder having very fine averge Snyder-Graff grain size comprising loading the powder in layers into a container formed from metal having a lower resistance to deformation than the metal of the billet, compacting each layer of metal by a high energy rate forming ram to a level of about 3×10 6 psi, adjusting the thickness and number of layers so that the powder in the container receives total energy at a level of at least 18×10 6 psi, covering the powder so compacted with an inner plate not attached to the container, covering the inner plate with

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗