Abstract
Manufacture of vitreous carbon bodies in which thermoplastic materials containing aromatic groups are formed into bodies, are thermally stabilized by irradiation with ionizing radiation and are carbonized by heating them in an inert atmosphere.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Method for the manufacture of vitreous carbon bodies from thermoplastic materials, which comprises, forming a thermoplastic material containing aromatic groups selected from the group consisting of polyphenylene oxide, polysulfone, polyether sulfone and polyether ether ketone into a body, irradiating the body with beta rays with an energy dose of at least 1 MJ/kg at a temperature below the softening temperature of the material and carbonizing the body by heating in an inert atmosphere to a temperature of at least 800° C.
- Claim 2Depends on #1
Method according to claim 1, wherein the thermoplastic material body is irradiated with an energy dose which is applied in steps.
- Claim 3Depends on #1
Method according to claim 1, wherein the body is irradiated with an energy dose insufficient for complete cross-linking.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (2)
- Polymer Letters, John Willey & Sons, Inc., vol. 8, pp. 121 126 (1970).
- Polymer Letters, John Willey & Sons, Inc., vol. 8, pp. 121-126 (1970).