Patents
US 4,698,103 A#6025021 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing dual phase strip steel and steel strip manufactured by the method

15Forward Citations (#6025021 Global)
0.4/yrCitation Velocity (#20889144 Global)
5.89Citation PageRank (#2536304 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In a method of manufacturing a dual phase steel a strip of thickness 0.1 to 0.5 mm from an unalloyed low C, low Mn steel composition of 0.02-0.15% C and 0.15-0.50% Mn, which method includes continuous annealing, a flat product can be obtained without strip fracture if (a) the strip is heated to not above 770° C. in the A 1 -A 3 region of the iron-carbon diagram region and thereafter (b) the strip is cooled sufficiently rapidly that austenite is at least partly converted to martensite and/or bainite, the cooling rate is such that the value P=d.V where d is strip thickness in mm and V is average cooling rate in °C/sec from 700° C. to 300° C., is in the range 20 to 900 and the time interval between the end of step (a) and the beginning of step (b) is less than 4 seconds.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a dual phase steel in the form of a strip of thickness in the range 0.1 to 0.5 mm from an unalloyed low C, low Mn steel composition having by weight 0.02-0.15% C 0.15-0.50% Mn comprising the steps of hot rolling cold rolling continuous annealing the said continuous annealing comprising (a) heating the strip to a temperature not exceeding 770° C. in the A 1 -A 3 region of the iron-carbon diagram and soaking it at said temperature and thereafter (b) cooling the strip at a rate sufficiently rapid that austenite is at least partly converted to martensite

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Metals Handbook, Ninth Edition, vol. 5, Surface Cleaning, Finishing and Coating, pp. 351, 471, 497.