Thermoplastic moulding compositions based on polyalkylene terephthalate and polymer and a process for the production thereof
Abstract
Polyalkylene terephthalates which contain a fluorinated polyolefin in addition to a polymer having a glass transition temperature of less than -30° C., are very tough, exhibit good stability to thermal shaping and hardness, and have a high modulus of elasticity and improved stress/strain behavior.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermoplastic moulding composition comprising A. from 65 to 99% by weight, based on the sum of A+B, of polybutylene terephthalate and B. from 1 to 35% by weight, based on the sum A+B, of a graft copolymer wherein the graft copolymer is comprised of from 15 to 60%, by weight of the graft copolymer, of a graft monomer selected from styrene, α-methylstyrene, acrylonitrile, C 1 -C 8 alkylacrylates, C 1 -C 8 alkylmethacrylates, hydroxy-C 2 14 C 8 -alkylacrylates, hydroxy-C 2 -C 8 -alkylmethacrylates, epoxy-C 2 -C 8 -alkylacrylates and epoxy-C 2 -C 8 -alkylmethacrylates grafter onto
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗