Method of making electrolytic capacitor anodes
Abstract
A powder of a film-forming metal, such as tantalum, is combined with a binder of polyethylene oxide and ammonium carbonate. The powder-binder combination is pressed to form an anode body and then heated to about 300° C. for about 4 hours to remove the binder. The polyethylene oxide is a superior binding agent producing anodes of high porosity and strength. The ammonium carbonate reacts with liquid polyethylene oxide to release large quantities of gas which sweeps the polyethylene oxide out of the anode pores, resulting in an unusually small amount of binder residue and yielding capacitors with low d.c. leakage.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 17.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of making an anode for an electrolytic capacitor, comprising the steps of: providing a powder comprised of a film-forming metal, polyethylene oxide, and ammonium carbonate; pressing the powder to form an anode body; and heating the anode body to remove the polyethylene oxide and ammonium carbonate.
- Claim 2Depends on #1
The method of claim 1 wherein said step of heating comprises heating to at least the melting range of polyethylene oxide.
- Claim 3Depends on #2
The method of claim 2 wherein said step of heating comprises heating to a temperature between 50° C. and 300° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗