Patents
US 4,663,418 A#15232886 Most CitedExpiredUnited States (USPTO)Utility

Novel calcium hydroxide catalyzed phenolic resin binder and method

7Forward Citations (#15232886 Global)
0.2/yrCitation Velocity (#35134694 Global)
1.77Citation PageRank (#17648448 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An improved moisture-stable phenolic resin binder with calcium ions from the catalyst complexed with the phenolic resin and a process for its preparation and laminate boards with the said binder as the binding agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A proces for the preparation of a moisture-stable phenolic resin binder comprising condensing a phenol and formaldehyde in an aqueous media in the presence of calcium hydroxide as catalyst to form a condensation product, cooling the reaction mixture after the condensation to 10° to 20° C., adjusting the pH of the reaction mixture to 8.5 to 10.5 by addition of a base and then adding 0.8 to 2.0 moles of sulfate ions per mol of the calcium ions while maintaining the pH in the range of 8.5 to 10.5.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the molar ratio of phenol to formaldehyde is 1:1.3 to 1:4.0.

  3. Claim 3Depends on #1

    The process of claim 1 wherein the amount of calcium hydroxide is 0.5 to 10.0% by weight based on the phenolic resin.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗