Abstract
A method of coating a substrate with a thin film of a polymer of predetermined porosity comprises depositing the thin film on the substrate from a non-gelled solution comprising at least one hydrolyzable metal alkoxide of a polymeric network forming cation, water, an alcohol compatible with the hydrolysis and the polymerization of the metal alkoxide, and an acid or a base, prior to depositing the film, controlling the structure of the polymer for a given composition of the solution exclusive of the acid or base component and the water component, (a) by adjusting each of the water content, the pH, and the temperature to obtain the desired concentration of alkoxide, and then adjusting the time of standing of the solution prior to lowering the temperature of the solution, and (b) lowering the temperature of the solution after the time of standing to about 15 degrees C. or lower to trap the solution in a state in which, after the depositing step, a coating of the desired porosity will be obtained, and curing the deposited film at a temperature effective for curing whereby there is obtained a thin film of a polymer of a predetermined porosity and corresponding pore size on the substrate
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 129.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of coating a substrate with a thin film of a polymer of predetermined porosity, comprising: depositing the thin film on the substrate from a dilute non-gelled solution comprising at least one hydrolyzable metal alkoxide of a polyermic network-forming cation, water, an alochol or other solvent compatible with the hydrolysis and the polymerization of the metal alkoxide, and an acid or a base, wherein the concentration of the alkoxide in said solution is about 1 to 12 equivalent weight %, and prior to the depositing said film, controlling the structure of said polymer for a given compo
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 129 total)
References Cited — Backward Prior Art (3)
Non-Patent Literature (5)
- Brinker et al., "A Comparison Between the Densification Kinetics of Colloidal and Polymeric Silica Gels," Mat. Res. Soc. Symp. Proc., 32 (1984), pp. 25--32.
- Brinker et al., "Comparison of Sol-Gel Derived Thin Films with Monoliths in Multicomponent Silicate Glass Systems," Thin Solid Films, 77 (1981), pp. 141-148.
- Brinker et al., "Conversion of Monolithic Gels to Glasses in a Multicomponent Silicate Glass System," J. Materials Sci., 16 (1981), pp. 1980-1988.
- Brinker et al., "Sol-Gel Derived Antireflective Coatings for Silicon," Solar Energy Matls, 5 (1981), pp. 159-172.
- Brinker et al., "Sol-Gel Derived Antireflective Coatings," Proc. of the Distributed Solar Collector Conference, Albuquerque, NM, Mar. 1983, pp. 68-80.