Tires
Abstract
A tire whose tread comprises as elastomer a styrene-butadiene or a styrene-isoprene co-polymer having a glass transition temperature above minus 50 DEG C., said composition having a rebound resilience of 55% or more. The glass transition temperature is preferably between minus 40 DEG C. and minus 25 DEG C. and the rebound resilience is preferably between 60% and 70%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 18.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A tire tread-forming elastomer composition containing as the elastomer a styrene-butadiene copolymer having a styrene content of not more than 40% and a glass transition temperature in the range from minus 45° C. to minus 20° C., said composition having a rebound resilience of about 55% to about 95% and conventional additives for tire tread-forming elastomer compositions including a vulcanizing agent.
- Claim 2Depends on #1
An elastomer composition according to claim 1, in which said glass transition temperature is in the range from minus 40° C. to minus 25° C.
- Claim 3Depends on #1
An elastomer composition according to claim 1, in which said rebound resilience is 60% or more.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 18 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- H. L. Hseih et al, Rubber Chem. Technol ., 74 (1970), p. 55, Table IX in conjunction with p. 56, paragraph 2.
- H. L. Hseih et al, Rubber Chem. Technol., 74 (1970), p. 55, Table IX in conjunction with p. 56, paragraph 2.
- K. H. Nordsiek, PTR Polymer Age, 4 (1973), pp. 332 333, 335 337.
- K. H. Nordsiek, PTR Polymer Age, 4 (1973), pp. 332-333, 335-337.
- R. S. Hanmer et al, Rubber Age , 96 (1964), pp. 73 77.