Chromium electroplating and bath therefor
Abstract
To a conventional chromium electroplating bath containing 450 g/l chromic acid CrO3 and 4.5 g/l sulphuric acid H2SO4 are added 10 g/l of potassium perchlorate or potassium bromate or potassium iodate or mixtures thereof. Higher current densities may be used in electrodepositing chromium without impairing the quality.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A bath composition for chromium electroplating comprising CrO 3 in a concentration of from 200 g/l to 600 g/l, sulphate in a weight ratio SO 4 :CrO 3 of from 1:120 to 1:80, perchlorate in a weight ratio ClO 4 :CrO 3 of from 1:500 to 1:50, bromate in a weight ratio BrO 3 :CrO 3 of from 1:50 to 1:20, and metal cations equivalent to at least half the perchlorate plus bromate.
- Claim 2Depends on #1
A bath composition according to claim 1, wherein the perchlorate has a weight ratio ClO 4 :CrO 3 of from 1:200 to 1:80.
- Claim 3Depends on #1
A bath composition according to claim 1, wherein the metal cations are equivalent to substantially all the perchlorate plus bromate.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- R. M. Krishnan et al., Metal Finishing, pp. 55 61, Oct. 1981.
- R. M. Krishnan et al., Metal Finishing, pp. 55-61, Oct. 1981.