US 4,643,191 A#425072 Most CitedExpiredUnited States (USPTO)Utility

Crystalline copolymers of p-dioxanone and lactide and surgical devices made therefrom

75Forward Citations (#425072 Global)
1.9/yrCitation Velocity (#2249075 Global)
15.19Citation PageRank (#529001 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A crystalline copolymer is produced by first polymerizing p-dioxanone to form a mixture of monomer and homopolymer, and then adding lactide to this mixture and polymerizing to form a copolymer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 75.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Process for producing a crystalline copolymer of p-dioxanone and lactide which comprises subjecting a mixture of p-dioxanone homopolymer, p-dioxanone monomer, and lactide to an elevated temperature for a period of time sufficient to produce a crystalline copolymer of p-dioxanone and lactide.

  2. Claim 2Depends on #1

    Process of claim 1 which comprises the steps of: (a) polymerizing p-dioxanone monomer in the presence of a catalytically effective amount of a polymerization catalyst and an initiator to produce a first mixture of p-dioxanone homopolymer and p-dioxanone monomer; and (b) adding lactide to said first mixture to produce a second mixture, and subjecting said second mixture to an elevated temperature for a period of time sufficient to produce a crystalline copolymer of p-dioxanone and lactide.

  3. Claim 3Depends on #2

    The process of claim 2 whe