Abstract
Improved halided alumina catalysts are prepared by first calcining the gamma-alumina catalyst base at a temperature of 1300°-1800° F. The finished catalyst can be employed for olefin polymerization without need for refrigeration to control the exothermic heat of reaction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for the manufacture of a high-activity chlorided alumina catalyst suitable for olefin polymerization comprising: calcining a catalyst base consisting essentially of gamma alumina at a temperature within the range from about 1300° F. to about 1800° F. for from about 6 to about 16 hours, followed by contacting the calcined catalyst base with a chloriding agent.
- Claim 2Depends on #1
The process of claim 1 wherein the chloriding agent is carbon tetrachloride, employed at a concentration of about 4 wt. % in air for about 6 hours at a temperature of about 650° F.
- Claim 3Depends on #1
The process of claim 1 wherein the calcination step is conducted with a flowing stream of an inert gas.